Polymer Property : Viscosity = 650 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 350 - 650 cP
350 - 650 cP
15% solution in MEK
Lubrizol Advanced Materials Pearlstick® 45-40/05 Polycaprolactone based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: DIY, AutomotiveInformation provided by Merquinsa
Viscosity 350 - 650 cP

@Temperature 23.0 °C
350 - 650 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy
Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of..
Viscosity 350 - 650 cP

@Temperature 40.0 °C
350 - 650 cP

@Temperature 104 °F
Abatron AboCast/AboCure 8109-10
2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro..
Viscosity 450 - 650 cP
450 - 650 cP
blended
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..