Material Notes:
This product is a silver bearing, thermoplastic, acrylic, polymer paint designed primarily as a conductive electrode solder base for tantalum capacitors. Additionally, this material can be used as a general purpose conductive paint for printed circuit board repair and electromagnetic shielding applications. It possesses good rheological properties for either dip or paint applications. The cured film has excellent electrical and environmental stability both initially and upon aging. The material is readily soldered using conventional tin/lead/silver solders for external lead attachment.All information provided by Lord.
Physical Properties Metric English Comments
Viscosity 350 - 450 cP
350 - 450 cP
Component Elements Properties Metric English Comments
Silver, Ag 40 - 44 %
40 - 44 %
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 100 ohm
<= 100 ohm
Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes
Descriptive Properties Value Comments
Settling Rate (mm/hr) <=2
Solder Leach Resistance (cycles) >5
Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes; Tested in 62Sn/36Pb/2Ag solder at 205ºC
Solder Wetting (seconds) 2-3
Dried at 80ºC for 10 minutes then cured at 150ºC for 30 minutes; Tested in 62Sn/36Pb/2Ag solder at 205ºC