Material Notes:
Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMULS EL-620/LI is a biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 - 1.06 g/cc
0.0376 - 0.0383 lb/in³
RP-0064
pH 6.0 - 8.0
6.0 - 8.0
7% Solution; RP-0420
Viscosity 350 - 1000 cP
350 - 1000 cP
#3 SP @ 60 RPM; RP-0659
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
RP-0138
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clean, clear to slightly hazy liquid
RP-0064
Composition Potassium
<5 ppm, RP-1005
Sodium
<50 ppm, RP-1005
Neutralization Number <0.4 mg KOH/g
(pH 7), RP-0343
Saponification number 73-78 mg KOH/g
RP-0496