Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Epoxy Technology
Trade Name EPO-TEK®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of EPO-TEK® 320 that can be poured, potted or cast into shape.Information Provided by Epoxy Technology
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
Part B
1.20 g/cc
1.20 g/cc
Part A
Viscosity 350 - 650 cP

@Temperature 23.0 °C
350 - 650 cP

@Temperature 73.4 °F
100 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Tensile Modulus 1.84 GPa
266 ksi
Storage
Shear Strength 11.6 MPa
1680 psi
Lap
>= 35.2 MPa
>= 5100 psi
Die
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C
26.7 µin/in-°F
Below Tg
170 µm/m-°C
94.4 µin/in-°F
Above Tg
Maximum Service Temperature, Air 200 °C
392 °F
Continuous
300 °C
572 °F
Intermittent
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Continuous
-55.0 °C
-67.0 °F
Intermittent
Glass Transition Temp, Tg >= 55.0 °C
>= 131 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 397 °C
747 °F
Degradation Temperature
Optical Properties Metric English Comments
Transmission, Visible <= 1.0 %

@Wavelength 300 - 2500 nm
<= 1.0 %

@Wavelength 300 - 2500 nm
Spectral
Electrical Properties Metric English Comments
Volume Resistivity >= 2.00e+9 ohm-cm
>= 2.00e+9 ohm-cm
Dielectric Constant 11.35

@Frequency 1000 Hz
11.35

@Frequency 1000 Hz
Dissipation Factor 0.283

@Frequency 1000 Hz
0.283

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Pot Life 60 min
60 min
Shelf Life 12.0 Month

@Temperature 25.0 °C
12.0 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Black
Part A
Clear/Colorless
Part B
Consistency Smooth pourable liquid
Mix Ratio By Weight 10:2
Number of Components Two
Weight Loss 0.26%
200°C
0.52%
250°C
1.02%
300°C