Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 30 - 50 cP @Temperature 25.0 °C |
30 - 50 cP @Temperature 77.0 °F |
Uncured |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Viscosity | 30 cP | 30 cP | |
Resinlab® CYNERGY CA6003 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 30 cP | 30 cP | |
Resinlab® CYNERGY CA6202 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 30 cP | 30 cP | |
Resinlab® CYNERGY CA6302 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Viscosity | 30 cP | 30 cP | |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Viscosity | 30 - 50 cP @Temperature 25.0 °C |
30 - 50 cP @Temperature 77.0 °F |
Uncured |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Viscosity | 30 cP | 30 cP | |
Resinlab® CYNERGY CA6803 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 30 - 70 cP | 30 - 70 cP | |
Huntsman Araldite XU 396 Reactive Diluent Weight per Epoxide (EEW, g/eq) 416 to 588. Max color is 13.Comments/Applications: Reactive diluent based on Cashew Nut Shell Liquid (CNSL). Very low volatility for high solids and solvent free coa.. |
|||
Viscosity | 30 - 70 cP | 30 - 70 cP | |
Huntsman HY 2963 Cycloaliphatic Amine Approx. H+ equivalent weight 85. Mix Ratio with GY 6010 is 45.Comments/Applications: Phenol-free version of HY 2964. Mortar and floor repair, sewage treatment plants, commercial and industrial fl.. |
|||
Viscosity | 30 cP | 30 cP | |
Lord Adhesives 5000 Fast Setting, High Elasticity, Low Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 30 - 70 cP | 30 - 70 cP | NOV QC 020 |
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 30 - 70 cP | 30 - 70 cP | Part B |
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis.. |
|||
Viscosity | 30 - 50 cP | 30 - 50 cP | |
Chesterton 415 Concrete Sealer Chesterton® 415 Concrete Sealer is a high gloss, fast penetrating coating which forms a polymeric seal over surfaces to which it is applied. When used on porous surfaces such as concrete floors, wa.. |
|||
Viscosity | 30 cP | 30 cP | |
Elmer's Products Aron Alpha® 231F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Viscosity | 30 - 60 cP @Temperature 60.0 °C |
30 - 60 cP @Temperature 140 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Viscosity | 30 - 80 cP | 30 - 80 cP | |
Beijing Ranger Chem 6690-3 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 30 cP | 30 cP | |
Aremco Ceramabind™ 643-2 High Temperature Inorganic Binder Excellent for formulating thin coatings that set at room temperature and can be raised rapidly to high temperatures |
|||
Viscosity | 30 - 90 cP @Temperature 25.0 °C |
30 - 90 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT CL-27 MDI Isocyanate Description of product: It is a carbo-diimide modified 4,4`-diphenyl-methane-diisocyanate.Field of application: With suitable polyols it can be used as isocyanate component for producing microcellul.. |
|||
Viscosity | 30 cP | 30 cP | A Component; ASTM D1824 |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |
|||
Viscosity | 30 cP | 30 cP | B Component; ASTM D1824 |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |