Polymer Property : Viscosity = 90 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 2011 Cyanoacrylate, gel
PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and..
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Viscosity 70 - 90 cP

@Temperature 25.0 °C
70 - 90 cP

@Temperature 77.0 °F
Uncured
Permabond 920 Cyanoacrylate, High temperature
PERMABOND® 920 is the original allyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. PERMAB..
Viscosity 40 - 90 cP
40 - 90 cP
NOV QC 020
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Viscosity 30 - 90 cP

@Temperature 25.0 °C
30 - 90 cP

@Temperature 77.0 °F
BorsodChem ONGRONAT CL-27 MDI Isocyanate
Description of product: It is a carbo-diimide modified 4,4`-diphenyl-methane-diisocyanate.Field of application: With suitable polyols it can be used as isocyanate component for producing microcellul..