Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond 105 Cyanoacrylate, for difficult rubbers

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond 105 Cyanoacrylate, for difficult rubbers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates ideal adhesives for high speed production lines. Features & Benefits: Natural and synthetic rubber bonding Ideal for hard to bond plastics Ease of use – no mixing or heat cure Bonds most materials 100% reactive, no solvents Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 30 - 50 cP

@Temperature 25.0 °C
30 - 50 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength >= 5.00 MPa
>= 725 psi
PC, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
6.00 - 8.00 MPa
870 - 1160 psi
Aluminum, Shear; ISO 4587
6.00 - 8.00 MPa
870 - 1160 psi
Zinc, Shear; ISO 4587
12.0 - 14.0 MPa
1740 - 2030 psi
Phenolic, Shear; ISO 4587
18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.167 min
0.00139 - 0.00278 hour
Buna N Rubber, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
Phenolic, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
PVC, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
ABS, handling time
0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
<= 0.333 min
<= 0.00556 hour
EPDM, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.1
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Users viewing this material also viewed the following: