Material Notes:
Description of product: It is a carbo-diimide modified 4,4`-diphenyl-methane-diisocyanate.Field of application: With suitable polyols it can be used as isocyanate component for producing microcellular elastomers, RIM elastomers, coatings and casting elastomers. Together with high molecular weight and reactive polyols it is suitable for producing prepolymers which can be used for manufacturing flexible and semi-flexible integral foams.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Viscosity 30 - 90 cP

@Temperature 25.0 °C
30 - 90 cP

@Temperature 77.0 °F
Descriptive Properties Value Comments
Hydrolizable chlorine 0.01 max wt%
NCO Content, wt% 27.5 - 29.5