Huntsman Araldite XU 396 Reactive Diluent

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite XU 396 Reactive Diluent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 416 to 588. Max color is 13.Comments/Applications: Reactive diluent based on Cashew Nut Shell Liquid (CNSL). Very low volatility for high solids and solvent free coatings and floorings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 30 - 70 cP
30 - 70 cP