Polymer Property : Viscosity = 60 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 35 - 60 cP
35 - 60 cP
ND Industries 306 Surface Insensitive Instant Superglue
Low viscosity for difficult to bond rubber compounds
Viscosity 35 - 60 cP
35 - 60 cP
3
ND Industries SuperGlue Ethyl 395
General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen..
Viscosity 20 - 60 cP
20 - 60 cP
Huntsman HY 1341 Cycloaliphatic Amine
Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Low viscosity, modified amine for fast cure, resistant to acids, alkali, solvents. Mortar and floor repair, s..
Viscosity 25 - 60 cP
25 - 60 cP
Huntsman Tactix 742 Epoxy
Weight per Epoxide (EEW, g/eq) 150 to 170.Comments/Applications: Trifunctional epoxy with excellent Tg and thermal stability in the cured state.Data provided by Ciba Specialty Chemicals.Ciba Special..
Viscosity 25 - 60 cP
25 - 60 cP
Huntsman Tactix 742 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 150 to 170.Comments/Applications: Trifunctional epoxy with excellent Tg and thermal stability in the cured state.Data provided by Ciba Specialty Chemicals.Ciba Special..
Viscosity 35 - 60 cP

@Temperature 25.0 °C
35 - 60 cP

@Temperature 77.0 °F
Mixed
Trelleborg Emerson & Cuming Eccobond® 11 Heat Cure Catalyst
Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to ..
Viscosity 30 - 60 cP

@Temperature 60.0 °C
30 - 60 cP

@Temperature 140 °F
Abatron AboCast/AboCure 8109-10
2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro..