3M Scotch-Weld™ MC5 Metal Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ MC5 Metal Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low viscosity cyanoacrylate primarily used for bonding smooth, even, close fitting parts. It is a wicking type cyanoacrylate that can be used in preassembled parts. It has been tested and passed the requirements of Commercial Item Description A-A-3097, Type 1, Class 1 (formerly MIL-A-46050C).Information provided by 3M
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Viscosity 2.0 - 5.0 cP
2.0 - 5.0 cP
U-Tube IC-C45
Mechanical Properties Metric English Comments
Shear Strength 21.4 MPa
3100 psi
Overlap, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.250 - 0.583 min
0.00417 - 0.00972 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid