Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.0 - 4.0 cP @Temperature 20.0 °C |
3.0 - 4.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-03 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 3.0 - 4.0 cP @Temperature 20.0 °C |
3.0 - 4.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-03 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 2.0 - 4.0 cP | 2.0 - 4.0 cP | |
Oceanchem Group Tri-isobutyl Phosphate (TIBP) Molecular Formula: C12H27O4PCas No.: 126-71-6Chemical Properties: Ester property, it can be hydrolyzed in basic condition.Hazardous Features: It can be fired in heat, fire and oxidation condition, a.. |
|||
Viscosity | 2.0 - 4.0 cP @Temperature 25.0 °C |
2.0 - 4.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |