Material Notes:
PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers are also rapidly bonded. The fast cure minimizes the occurrence of frosting and fogging. The wicking viscosity of this product makes it ideal for post-assembly application. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND® cyanoacrylates the ideal adhesives for high speed production lines. Features & Benefits: Extremely fast setting Rapid development of high strength Ease of use – no mixing or heat cure Surface insensitive 100% reactive, no solvents Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 2.0 cP

@Temperature 25.0 °C
2.0 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.0333 - 0.0500 min
0.000556 - 0.000833 hour
Steel, handling time
0.0333 - 0.0500 min
0.000556 - 0.000833 hour
Buna Rubber, set time
0.0333 - 0.0500 min
0.000556 - 0.000833 hour
Phenolic, set time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.05
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C