Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3.0 - 10 cP @Temperature 25.0 °C |
3.0 - 10 cP @Temperature 77.0 °F |
Uncured |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Viscosity | 8.0 - 10 cP @Temperature 20.0 °C |
8.0 - 10 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-08 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 2.0 - 10 cP | 2.0 - 10 cP | |
3M Pronto™ CA-40 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with.. |