Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 16000 - 18000 cP @Temperature 25.0 °C |
16000 - 18000 cP @Temperature 77.0 °F |
Uncured |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Viscosity | 10000 - 18000 cP | 10000 - 18000 cP | |
Lord Adhesives 305 General Purpose, Medium Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 10000 - 18000 cP | 10000 - 18000 cP | |
Lord Adhesives 307 General Purpose, Medium Viscosity Hardener for Lord 305-1 Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 12000 - 18000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
12000 - 18000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2041206P2 Gold Polymer Electrode Paste Gold paste is a screen printable gold polymer paste designed as a working electrode in electrochemical biosensors. This is used as a working electrode in medical diagnostics, environmental sensor a.. |
|||
Viscosity | 11000 - 18000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
11000 - 18000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2060217P3 Lead-free Silver Topcoat Ink This product is a Lead free version of C70709D21. Silver Ink C2060217D3 is designed as a top coat for Silver Zinc Ink C2061103D7 printed on PTC ceramics. Screen Printing Equipment: semi-automatic, m.. |
|||
Viscosity | 11000 - 18000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
11000 - 18000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2100217D1 Aluminium for PTC paste Aluminium Ink designed to give good ohmic contact on to barium titanate PTC components. This product is particularly good where large volumes of PTC components are being processed in belt furnaces .. |
|||
Viscosity | 10000 - 18000 cP | 10000 - 18000 cP | Part A |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Viscosity | 14000 - 18000 cP | 14000 - 18000 cP | Mixed system |
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr.. |
|||
Viscosity | 15000 - 18000 cP @Temperature 23.0 °C |
15000 - 18000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2101 is a two component, thixotropic, electrically conductive adhesive. It may be used for circuit assembly and semiconductor applications. Advantages & Application .. |
|||
Viscosity | 13000 - 18000 cP @Temperature 23.0 °C |
13000 - 18000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and f.. |
|||
Viscosity | 14000 - 18000 cP | 14000 - 18000 cP | mixed compound |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |