Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 13000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
13000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Viscosity | 13000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
13000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Viscosity | 13000 - 15000 cP | 13000 - 15000 cP | |
Huntsman MY 9634 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistan.. |
|||
Viscosity | 13000 - 17000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
13000 - 17000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2100303D2 Aluminium Paste This product has been designed as a low temperature fireable aluminum paste. It is a screen printing ink for coating barium titanate PTC ceramic substrates. Screen Printing Equipment: semi-automati.. |
|||
Viscosity | 13000 - 17000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
13000 - 17000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2081009D6 Polymer Dielectric Transparent green colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The .. |
|||
Viscosity | 13000 cP | 13000 cP | Dynamic |
Solvay Chemicals DIGLYCEROL Diglycerol is a clear viscous liquid very similar to glycerol. It has a higher molecular weight than glycerol and is less volatile. It is water soluble and can be combined with aqueous systems.EINEC.. |
|||
Viscosity | 13000 cP | 13000 cP | Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2 |
Formosa Plastics Formolon® 34 PVC PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t.. |
|||
Viscosity | <= 13000 cP | <= 13000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals HyTemp® 4051EP AR Polyacrylate Elastomer HyTemp 4051EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Easy processing version of.. |
|||
Viscosity | 13000 cP @Temperature 25.0 °C |
13000 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for .. |
|||
Viscosity | 13000 cP | 13000 cP | dynamic |
Dow Corning SILASTIC® LSR 9151-200P PARTS A&B A solventless, 2-part liquid silicone rubber available in white which has excellent water and chemical resistance, low and high temperature stability from -60 to 200 C (-76 to 392 F) and rapid cure .. |
|||
Viscosity | 13000 - 18000 cP @Temperature 23.0 °C |
13000 - 18000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and f.. |
|||
Viscosity | 13000 cP | 13000 cP | Mixed |
Armstrong A-5/E Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Viscosity | 13000 cP | 13000 cP | |
3M Jet-Weld™ TE-031 Adhesive A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly. Extrudable grade with fast set time ideal for bonding a wide variety of plastics, i.. |
|||
Viscosity | 13000 - 15000 cP | 13000 - 15000 cP | |
Beijing Ranger Chem SM828R Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 13000 cP @Temperature 177 °C |
13000 cP @Temperature 350 °F |
Typical |
Bostik 6390 Good Heat Resistance, General Purpose EVA Glue Stick Bostik 6390 Good Heat Resistance, General Purpose EVA Glue StickGood heat resistance. Bonds plastics, wood, porous materials. General purpose adhesion. |
|||
Viscosity | 13000 cP | 13000 cP | dynamic |
Dow Corning 3110 SILICONE RUBBER ENCAPSULANT Two-part, white, condensation cure, moderate flow, general purpose encapsulant, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |
|||
Viscosity | 13000 cP @Temperature 25.0 °C |
13000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 2651MM/11 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Viscosity | 13000 cP @Shear Rate 100 1/s, Temperature 25.0 °C |
13000 cP @Shear Rate 100 1/s, Temperature 77.0 °F |
Haake VT550 cone and plate viscometer (PK1.1°) |
Gwent Electronic Materials C2010809D3 Silver Ink Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma.. |