Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.0107 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.0103 cm/cm Grade Count:80
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Linear Mold Shrinkage, Transverse 0.00110 - 0.0180 cm/cm
0.00110 - 0.0180 in/in
Average value: 0.00975 cm/cm Grade Count:44
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0180 cm/cm
0.00200 - 0.0180 in/in
Average value: 0.0113 cm/cm Grade Count:15
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Linear Mold Shrinkage, Transverse 0.0137 - 0.0180 cm/cm
0.0137 - 0.0180 in/in
Average value: 0.0146 cm/cm Grade Count:3
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage, Transverse 0.00400 - 0.0180 cm/cm
0.00400 - 0.0180 in/in
Average value: 0.0120 cm/cm Grade Count:9
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Linear Mold Shrinkage, Transverse 0.00950 - 0.0180 cm/cm
0.00950 - 0.0180 in/in
Average value: 0.0126 cm/cm Grade Count:4
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0180 cm/cm
0.0100 - 0.0180 in/in
Average value: 0.0139 cm/cm Grade Count:101
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..