Polymer Property : Linear Mold Shrinkage, Transverse = 0.00200 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00467 cm/cm Grade Count:3
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00592 cm/cm Grade Count:24
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cm
0.00200 - 0.00600 in/in
Average value: 0.00333 cm/cm Grade Count:3
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00640 cm/cm
0.00200 - 0.00640 in/in
Average value: 0.00570 cm/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00400 cm/cm
0.00200 - 0.00400 in/in
Average value: 0.00283 cm/cm Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00700 cm/cm
0.00200 - 0.00700 in/in
Average value: 0.00429 cm/cm Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00750 cm/cm
0.00200 - 0.00750 in/in
Average value: 0.00442 cm/cm Grade Count:15
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00557 cm/cm Grade Count:7
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0120 cm/cm
0.00200 - 0.0120 in/in
Average value: 0.00545 cm/cm Grade Count:34
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00545 cm/cm Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0100 cm/cm
0.00200 - 0.0100 in/in
Average value: 0.00740 cm/cm Grade Count:20
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage, Transverse 0.00200 - 0.100 cm/cm
0.00200 - 0.100 in/in
Average value: 0.0150 cm/cm Grade Count:30
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0122 cm/cm
0.00200 - 0.0122 in/in
Average value: 0.00844 cm/cm Grade Count:13
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0180 cm/cm
0.00200 - 0.0180 in/in
Average value: 0.0113 cm/cm Grade Count:15
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00544 cm/cm Grade Count:11
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0111 cm/cm Grade Count:94
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00600 cm/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0253 cm/cm
0.00200 - 0.0253 in/in
Average value: 0.0156 cm/cm Grade Count:62
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0130 cm/cm
0.00200 - 0.0130 in/in
Average value: 0.00812 cm/cm Grade Count:47
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0143 cm/cm Grade Count:17
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved