Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0227 cm/cm | 0.0100 - 0.0227 in/in | Average value: 0.0139 cm/cm Grade Count:9 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0198 cm/cm Grade Count:4 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0189 cm/cm Grade Count:61 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0210 cm/cm | 0.0100 - 0.0210 in/in | Average value: 0.0144 cm/cm Grade Count:14 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0150 cm/cm | 0.0100 - 0.0150 in/in | Average value: 0.0122 cm/cm Grade Count:6 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0400 cm/cm | 0.0100 - 0.0400 in/in | Average value: 0.0188 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0400 cm/cm | 0.0100 - 0.0400 in/in | Average value: 0.0197 cm/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0141 cm/cm Grade Count:3 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 cm/cm | 0.0100 in/in | Average value: 0.0100 cm/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0140 cm/cm | 0.0100 - 0.0140 in/in | Average value: 0.0111 cm/cm Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0180 cm/cm | 0.0100 - 0.0180 in/in | Average value: 0.0139 cm/cm Grade Count:101 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |