Polymer Property : Linear Mold Shrinkage, Transverse = 0.0137 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, ..
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
Plastcom SLOVAMID 66 C 15 MI PA66, 15% mineral filling
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
Plastcom SLOVAMID 66 T 15 MI PA66, 15% mineral filling
FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produc..
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
STN 64 0808
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled
FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove..
Linear Mold Shrinkage, Transverse 0.0137 - 0.0180 cm/cm
0.0137 - 0.0180 in/in
Average value: 0.0146 cm/cm Grade Count:3
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage, Transverse 0.0137 - 0.0141 cm/cm
0.0137 - 0.0141 in/in
Average value: 0.0139 cm/cm Grade Count:3
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..