Linear Mold Shrinkage, Transverse 0.00110 - 0.0180 cm/cm
0.00110 - 0.0180 in/in
Average value: 0.00975 cm/cm Grade Count:44
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Linear Mold Shrinkage, Transverse 0.00110 - 0.0207 cm/cm
0.00110 - 0.0207 in/in
Average value: 0.00514 cm/cm Grade Count:5
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Linear Mold Shrinkage, Transverse 0.00110 - 0.0300 cm/cm
0.00110 - 0.0300 in/in
Average value: 0.0132 cm/cm Grade Count:94
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage, Transverse 0.00110 - 0.0263 cm/cm
0.00110 - 0.0263 in/in
Average value: 0.0164 cm/cm Grade Count:15
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..