Polymer Property : Linear Mold Shrinkage, Transverse = 0.0100 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0100 - 0.0227 cm/cm
0.0100 - 0.0227 in/in
Average value: 0.0139 cm/cm Grade Count:9
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0198 cm/cm Grade Count:4
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0189 cm/cm Grade Count:61
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0210 cm/cm
0.0100 - 0.0210 in/in
Average value: 0.0144 cm/cm Grade Count:14
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0150 cm/cm
0.0100 - 0.0150 in/in
Average value: 0.0122 cm/cm Grade Count:6
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0188 cm/cm Grade Count:10
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0197 cm/cm Grade Count:12
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0141 cm/cm Grade Count:3
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage, Transverse 0.0100 cm/cm
0.0100 in/in
Average value: 0.0100 cm/cm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0140 cm/cm
0.0100 - 0.0140 in/in
Average value: 0.0111 cm/cm Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0180 cm/cm
0.0100 - 0.0180 in/in
Average value: 0.0139 cm/cm Grade Count:101
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..