Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00 - 0.0010 cm/cm

@Thickness 3.17 mm
0.00 - 0.0010 in/in

@Thickness 0.125 in
Ovation Polymers RIGITRON 30530 GF Polyester, 30% Glass Reinforced
Polyester – 30 % Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Va..
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.17 mm
0.00 - 0.0020 in/in

@Thickness 0.125 in
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var..
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4401R PPC+PC
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4404 PPC+PC
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.20 mm
0.00 - 0.0020 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Linear Mold Shrinkage, Transverse 0.00 cm/cm
0.00 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.00 - 0.0040 cm/cm
0.00 - 0.0040 in/in
ASTM D955
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Linear Mold Shrinkage, Transverse 0.00 - 0.0060 cm/cm
0.00 - 0.0060 in/in
ASTM D955
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ..
Linear Mold Shrinkage, Transverse 0.00 - 0.0060 cm/cm
0.00 - 0.0060 in/in
ASTM D955
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
Linear Mold Shrinkage, Transverse 0.00 - 0.020 cm/cm
0.00 - 0.020 in/in
Flame Bar; ASTM D955
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Linear Mold Shrinkage, Transverse 0.00 cm/cm

@Temperature 240 °C
0.00 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Linear Mold Shrinkage, Transverse 0.00 cm/cm
0.00 in/in
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer
DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent soft touch feel a..
Linear Mold Shrinkage, Transverse 0.00 cm/cm
0.00 in/in
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer
DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent soft touch feel a..
Linear Mold Shrinkage, Transverse 0.00 cm/cm
0.00 in/in
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer
DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent soft touch feel a..