Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 830-48/1-AY-ERYB Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 830-48/1-AY-ERYB Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.53 g/cc
1.47 - 1.53 g/cc
ASTM D 792
ASTM Color -1.29 - 0.31
-1.29 - 0.31
Color B, ME 12
-0.910 - 0.69
-0.910 - 0.69
Color A, ME 12
26.87 - 28.47
26.87 - 28.47
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 39.2 MPa
>= 5690 psi
ASTM D 638
Descriptive Properties Value Comments
Application General Purpose Profiles
Copyright © lookpolymers.com All Rights Reserved