Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman SCHULAMID® 66 MK4015 40% Glass Fiber/Mineral Reinforced 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.175 mm
0.0050 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 129.88 MPa
18837 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 169.84 MPa
24633 psi
ASTM D790
Flexural Modulus 8.9915 GPa
1304.1 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.81 J/cm
9.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
489 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 290 - 310 °C
554 - 590 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
Users viewing this material also viewed the following: