Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: cured silicone rubber
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 229 microns
9.00 mil
side 1; Arlon SQA-TMS-003
229 microns
9.00 mil
side 2; Arlon SQA-TMS-003
356 microns
14.0 mil
substrate; Arlon SQA-TMS-003
813 microns
32.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
silicone property; ASTM D2240
Tensile Strength, Ultimate 6.21 MPa
900 psi
silicone property; ASTM D412
Elongation at Break 350 %
350 %
silicone property; ASTM D412
Tear Strength 44.5 kN/m
254 pli
Fill; Arlon SQA-TMS-026
51.9 kN/m
296 pli
Warp; Arlon SQA-TMS-026
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 28.0 kV/mm
712 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red