Material Notes:
Description: SEQUEL® 1823 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperature range. This material provides excellent processability and dimensional stability. Applications: Body panels, bumper beams, energy absorbers, and brackets Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.74 GPa
252 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 25.0 J
18.4 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
25.0 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228