Michelman® SofTak® 326 Non-skid coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name SofTak®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® SofTak® 326 Non-skid coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Non-skid coating.Usage: SofTak® 326 is an excellent nonskid coating that also has a fair amount of water resistance. It is often used on slip/tier sheets or a variety of other applications that require a high COF surface. Application Data: SofTak® 326 is rod and blade coater applicable.Softak® is typically used for: Slip or tier sheets to prevent slipping of palletized loads, boxes and furniture; Coated paper used as temporary flooring where skid resistance is critical; Protective floor mats for highly-polished surfaces during moving phase; and Jewelry and perfume packagingInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
pH 8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity 200 - 600 cP
200 - 600 cP
Spindle # 3, rpm 60
Viscosity Measurement 11 - 16
11 - 16
[sec], EZ cup, Cup # 3
Descriptive Properties Value Comments
Appearance White, opaque liquid
Solids Type Polymer