Michelman® Nomar® 70AFN Non-abrasive paper coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Nomar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Nomar® 70AFN Non-abrasive paper coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Non-abrasive paper coatingUsage: Nomar® 70AFN is a water based, gluable, non-abrasive coating generally used to provide abrasion protection for gas flushed food packaging or small appliances. It is typically applied to the inner package or to shippers and partitions. It contains no fluorocarbon or PFOA. Nomar® 70AFN is gluable with both cold set and hot melt glues.Application Data: Nomar®70AFN can be applied by either rod or blade coater at the wet end of the corrugator and by blade at the dry end.Nomar® is typically used on: Snack food packages to prevent pinholing; Packaging for automotive parts such as headlight lenses and plastic body parts to prevent scratching; Partitions inside boxes so that more items can be packed into each box without risk of abrasion; and Cornerposts used in appliances boxes to reduce surface contact between the appliance and the boxFood Contact Information when manufactured in the USA: FDA: 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
pH 8.5 - 100
8.5 - 100
Brookfield Viscosity 100 - 300 cP
100 - 300 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Milky white liquid
Solids Type Polymer