Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Ultimate 16.5 MPa
2400 psi
ASTM D412
Tensile Strength, Yield 1.45 MPa
210 psi
at 100%; ASTM D412
Tear Strength 26.3 kN/m
150 pli
die C; ASTM D624
Compression Set 50 - 60 %
50 - 60 %
ASTM D395