BCC Products BC 8660E Urethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 8660E Urethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC8660E is a multi-purpose elastomer that can perform many functions. Special product characteristics are: excellent use for molds for casting of concrete and plaster, resists moisture absorption, does not contain MOCA, MDA, TDI or MDI, very easy to use and cures at room temperature.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
hardener
1.05 g/cc
1.05 g/cc
cured density
1.07 g/cc
1.07 g/cc
resin
Brookfield Viscosity 2500 cP
2500 cP
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 62
58 - 62
Tensile Strength, Ultimate 11.20 MPa
1625 psi
Elongation at Break 700 %
700 %
Tear Strength 35.1 kN/m
200 pli
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
full cure
Pot Life 25 min

@Temperature 25.0 °C
25 min

@Temperature 77.0 °F
work life
Descriptive Properties Value Comments
Mix Ratio 100:55 by weight (resin/hardener)