Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
Noble Polymers Forte™ 12HPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ISO 1183 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Specific Gravity | 0.926 - 0.931 g/cc | 0.926 - 0.931 g/cc | ASTM D1505 |
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D1505 |
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac.. |
|||
Specific Gravity | 0.926 g/cc | 0.926 g/cc | ASTM D792 |
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA.. |