A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA Regulation CFR 177.1520(c)3.1.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
ESCR 100% Igepal® >= 50 hour
>= 50 hour
Condition C; ASTM D1693
Melt Index of Compound 33 g/10 min

@Load 2.16 kg,
Temperature 190 °C
33 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Yield 13.1 MPa
1900 psi
2"/min; ASTM D638
Elongation at Break 120 %
120 %
2"/min; ASTM D638
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
Processing Properties Metric English Comments
Melt Temperature 95.0 °C
203 °F
Users viewing this material also viewed the following: