Physical Properties Metric English Comments
Specific Gravity 0.926 g/cc
0.926 g/cc
ISO 1183
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..
Specific Gravity 0.926 g/cc
0.926 g/cc
ISO 1183
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
Noble Polymers Forte™ 12HPP093 Nanocomposite
Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica..
Specific Gravity 0.926 g/cc
0.926 g/cc
ISO 1183
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene
Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h..
Specific Gravity 0.926 - 0.931 g/cc
0.926 - 0.931 g/cc
ASTM D1505
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D1505
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film
This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac..
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D792
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..