Polymer Property : Specific Gravity = 0.931 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.926 - 0.931 g/cc
0.926 - 0.931 g/cc
ASTM D1505
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical