Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional packagingFood packagingConverter filmsInformation provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Specific Gravity 0.926 g/cc
0.926 g/cc
ASTM D1505
Water Vapor Transmission 1.03 g/m²/day
0.0663 g/100 in²/day
ASTM F1249
Oxygen Transmission Rate 4900 cc/m²/day
316 cc/100 in²/day
ASTM D3985
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 2750 ppm
2750 ppm
Slip Level 750 ppm
750 ppm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.12
0.12
ASTM D1894
Elmendorf Tear Strength, MD 8.86 g/micron
225 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 6.89 g/micron
175 g/mil
ASTM D1922
Dart Drop 2.95 g/micron
75.0 g/mil
ASTM D1709
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 115 %
115 %
at 60°; ASTM D523
Processing Properties Metric English Comments
Blow-up Ratio (BUR) 2.5
2.5