Barlog Plastics KEBAFLEX SG 60 HT A.01 black TPE-S, Shore A60, black

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX SG 60 HT A.01 black TPE-S, Shore A60, black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPE-SInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 5.70 MPa
827 psi
ISO 527-1
Elongation at Break 315 %
315 %
ISO 527-1
Descriptive Properties Value Comments
Resin Type TPE-S