Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | |
Plastcom SLOVALEN PH 52 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANAMID 66 AL220L2M Nylon 66, Impact Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Polymer Resources NY66-IM2 Impact Modified Nylon 66 Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 3.20 mm |
0.017 in/in @Thickness 0.126 in |
Transverse |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 80.0 mm |
0.017 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | <= 0.017 cm/cm | <= 0.017 in/in | Note 1 |
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Linear Mold Shrinkage | <= 0.017 cm/cm | <= 0.017 in/in | Note 1 |
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Samyang Triel® 5600 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5600 is an extrusion grade.Information provided by Samyang. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
|
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | Bayer Test |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | MD; ASTM D955 |
Aclo Accucomp Polyethylene HD0205L High Density |
|||
Linear Mold Shrinkage | 0.017 cm/cm | 0.017 in/in | ± 0.1 at 120°C; ASTM D1238 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | ASTM D955 |
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang. |