Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.10 - 1.14 g/cc
0.0397 - 0.0412 lb/in³
Average value: 1.12 g/cc Grade Count:5
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm
0.00300 - 0.00800 in/in
Average value: 0.00450 cm/cm Grade Count:3
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 - 119 MPa
4000 - 17300 psi
Average value: 57.1 MPa Grade Count:3
Elongation at Break 2.00 - 11.0 %
2.00 - 11.0 %
Average value: 4.14 % Grade Count:4
Flexural Yield Strength 49.6 - 162 MPa
7200 - 23500 psi
Average value: 89.6 MPa Grade Count:3
Flexural Modulus 1.90 - 4.28 GPa
276 - 621 ksi
Average value: 2.94 GPa Grade Count:4
Izod Impact, Notched 0.340 - 0.534 J/cm
0.637 - 1.00 ft-lb/in
Average value: 0.469 J/cm Grade Count:3
Izod Impact, Unnotched 0.600 - 7.21 J/cm
1.12 - 13.5 ft-lb/in
Average value: 3.41 J/cm Grade Count:4
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -20.0 - -20.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 8.00 kJ/m² Grade Count:1
8.00 - 8.00 kJ/m²

@Thickness 4.00 - 4.00 mm
3.81 - 3.81 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 8.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 60.0 - 60.0 kJ/m²

@Temperature -20.0 - -20.0 °C
28.6 - 28.6 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 60.0 kJ/m² Grade Count:1
60.0 - 60.0 kJ/m²

@Thickness 4.00 - 4.00 mm
28.6 - 28.6 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 60.0 kJ/m² Grade Count:1
Charpy Impact, Notched 1.50 - 1.50 J/cm²

@Temperature -20.0 - -20.0 °C
7.14 - 7.14 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 1.50 J/cm² Grade Count:1
1.50 - 1.50 J/cm²

@Thickness 102 - 102 mm
7.14 - 7.14 ft-lb/in²

@Thickness 4.00 - 4.00 in
Average value: 1.50 J/cm² Grade Count:1
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 - 100 °C
190 - 212 °F
Average value: 94.8 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 73.0 - 102 °C
163 - 215 °F
Average value: 86.8 °C Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 500000 ohm-cm Grade Count:4
Surface Resistance 3.00 - 1.00e+6 ohm
3.00 - 1.00e+6 ohm
Average value: 376000 ohm Grade Count:5