Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Particle Size | 2500 µm | 2500 µm | Cubical Shape |
DAK Americas Laser+® HS AD600A PET Product Description: Laser+® HS (AD600A) is designed for PET packaging by injection stretch blow-molding using commercial heat-set technology. This polymer was formulated for processes requiring fa.. |
|||
Particle Size | 2500 µm | 2500 µm | Cubical Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® HS CF746A (D53A) PET Product Description: Laser+® HS CF746A (D53A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technolo.. |
|||
Particle Size | 2500 µm | 2500 µm | Cubical Shape |
DAK Americas Laser+® MB912 PET Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr.. |
|||
Particle Size | 2500 µm | 2500 µm | Cubical Shape; DAK-QAR-SOP-0017 |
DAK Americas Laser+® W PJ002 F43A PET Product Description: Laser+® W PJ002 (F43A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology... |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Particle Size | >= 2500 µm | >= 2500 µm | |
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Particle Size | 2500 - 3500 µm | 2500 - 3500 µm | Average value: 2800 µm Grade Count:47 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Particle Size | 2500 µm | 2500 µm | Pellet Size |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |