Material Notes:
Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and film/sheet applications.Applications/UsesAPET film and sheetInjection molded containersPET Bottles 2 stage and single stage
Physical Properties Metric English Comments
Bulk Density 0.820 g/cc
0.0296 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 57.0 J/g
24.5 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1269
1.30 J/g-°C

@Temperature 80.0 °C
0.311 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.80 J/g-°C

@Temperature 200 °C
0.430 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.00 J/g-°C

@Temperature 280 °C
0.478 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 241 °C
466 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
TEPO-A-AN-G-GC-67
Color, CIE a* -3.8 to -0.8
VGAS-A-AN-G-RS-001
Color, CIE b* -2.3 to 1.7
VGAS-A-AN-G-RS-001
Color, CIE L* 78 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
VGAS-A-AN-G-GA-1
Pellet Shape Cylindrical