Material Notes:
VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and better bottle properties. CB11E is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with this polymer deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance.Applications/UsesCarbonated soft drink containersBeverage PackagingBottles
Physical Properties Metric English Comments
Bulk Density 0.830 g/cc
0.0300 lb/in³
Poured; ASTM D1895
0.880 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.80 - 0.84
0.80 - 0.84
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 60.0 J/g
25.8 BTU/lb
ASTM E793
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
ASTM E1269
1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
2.00 J/g-°C

@Temperature 200 °C
0.478 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.30 J/g-°C

@Temperature 280 °C
0.550 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 243 °C
469 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
TEPO-A-AN-G-GC-67
Color, CIE a* -3.16 to -0.16
VGAS-A-AN-G-RS-001
Color, CIE b* -2.2 to 1.6
VGAS-A-AN-G-RS-001
Color, CIE L* 76.8 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
VGAS-A-AN-G-GA-1
Pellet Shape Cubical