Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DAK Americas Laser+® HS AD600A PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer DAK Americas
Trade Name Laser+®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DAK Americas Laser+® HS AD600A PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Laser+® HS (AD600A) is designed for PET packaging by injection stretch blow-molding using commercial heat-set technology. This polymer was formulated for processes requiring faster crystallization rates, higher glass transition and melting points, but balancing injection molding cycles speed and superior container appearance. This product is produced in Zarate, Argentina and will be supplied to customers in the Mercosur regionApplication/Uses: Hot filling Bottles; Food packaging; and Packaging.Information provided by DAK Americas
Physical Properties Metric English Comments
Bulk Density 0.817 g/cc
0.0295 lb/in³
Poured; ASTM D1895
0.865 g/cc
0.0312 lb/in³
Vibrated; ASTM D1895
Particle Size 2500 µm
2500 µm
Cubical Shape
Viscosity Measurement 0.80 - 0.84
0.80 - 0.84
VGAS-A-AN-G-V-1 (or equivalent)
Descriptive Properties Value Comments
Color >74 CIE
L*, VGAS-A-AN-G-RS-0001
-3.1 - 0.9 CIE
b*, VGAS-A-AN-G-RS-0001
-3.3- -0.3 CIE
a*, VGAS-A-AN-G-RS-0001
Compounds <2 ppm
Acetaldehyde, VGAS-A-AN-G-GC-2
Fines <0.05%
VGAS-A-AN-G-GA-1 (or equivalent)