Material Notes:
Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damaging wavelengths of light, protecting the contents of the package. In addition, Vitiva PET allows brand owners to achieve uniquely shaped containers with extraordinary clarity thereby showcasing the contents of the package.Applications/UsesCosmeticsHealth and nutrition containersHousehold products containersPharmaceutical containersCustom bottlesHotfilled food and beverage containersPersonal careKey AttributesChemical compatibility with packaged goodsDrop-in replacement for standard PETExceptional drop impact strengthMeets FDA regulations for food contactUnlimited recyclabilityExcellent clarityExcellent oxygen gas barrierFDA-compliant UV light barrierVirtually unlimited bottle design freedom
Physical Properties Metric English Comments
Bulk Density 0.818 g/cc
0.0296 lb/in³
Poured; ASTM D1895
0.888 g/cc
0.0321 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.76 - 0.80
0.76 - 0.80
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 63.0 J/g
27.1 BTU/lb
ASTM E793
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
ASTM E1269
1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.50 J/g-°C

@Temperature 100 °C
0.359 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.80 J/g-°C

@Temperature 200 °C
0.430 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.00 J/g-°C

@Temperature 280 °C
0.478 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 247 °C
477 °F
Crystalline Peak Melting Point; ASTM D3418
Optical Properties Metric English Comments
UV Transmittance <= 7.0 %

@Thickness 0.229 mm,
Wavelength 370 nm
<= 7.0 %

@Thickness 0.00900 in,
Wavelength 370 nm
well-oriented bottle sidewalls; VCSC-A-AS-G-CA-0005
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* -1.5 ± 2.0
VGAS-A-AN-G-RS-001
Color, CIE b* 0.5 ± 1.7
VGAS-A-AN-G-RS-001
Color, CIE L* 77.8 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.1
Pellet Shape Cubical