DAK Americas Laser+® MB912 PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer DAK Americas
Trade Name Laser+®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DAK Americas Laser+® MB912 PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient processing and good overall bottle properties. This polymer is formulate to provide improved efficiencies in perform and bottle production while delivering a robust processing window. Bottles made with Laser+® MB912 deliver good CO2 barrier with continued excellent performance in creep and environmental stress-crack resistance.Key Attributes:Good performance in stress-crack resistanceHigh reheat capability that provides fast and efficient processing in stretch blow moldingGood CO2 barrierRobust processing windowApplication/Uses: Carbonated soft drink bottles and custom, edible oil, food, juices and personal care bottles and containers.Information provided by DAK Americas
Physical Properties Metric English Comments
Bulk Density 0.817 g/cc
0.0295 lb/in³
Poured; ASTM D1895
0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Cubical Shape
Viscosity Measurement 0.82 - 0.86
0.82 - 0.86
[dL/g], Intrinsic; DRAM-A-G-V-3
Thermal Properties Metric English Comments
Heat of Fusion 59.0 J/g
25.4 BTU/lb
DSC on the first heating cycle; ASTM E793
Specific Heat Capacity 1.00 J/g-°C

@Temperature 22.8 °C
0.240 BTU/lb-°F

@Temperature 73.0 °F
ASTM E1269
1.21 J/g-°C

@Temperature 80.0 °C
0.290 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.38 J/g-°C

@Temperature 100 °C
0.330 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.72 J/g-°C

@Temperature 200 °C
0.410 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
1.88 J/g-°C

@Temperature 280 °C
0.450 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Crystallization Temperature 245 °C
473 °F
DSC on second heating cycle, Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Color >74.5 CIE
L*, DRAM-A-G-RS-1
-4 - -1 CIE
b*, DRAM-A-G-RS-1
Compounds <3 ppm
Acetaldehyde, DRAM-A-G-GC-5
Fines <0.05%
DRAM-A-GA-1