Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | |
MarkeTech Repton EXP 386 Aluminum Titanate REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 Moldable Refractory Material Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | |
Sharadaa Ceramics PHOSTCAST 90 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 001 Smart Cast Application Special Properties: Thermal Shock Slag ResistanceIndustry: FoundryApplication Areas: Foundry LaddleInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 004 Smart Cast Application Special Properties: Thermal Shock, Abrasion, Alkali ResistanceIndustry: SteelApplication: Lances, Launders, Riser TubesInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 006 Smart Cast Application Special Properties: Thermal Shock, Flame ErosionIndustry: Multi PurposeApplication: Burner Blocks all types of Thermal Shock ApplicationsInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | |
China Tungsten YG12X Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | |
Chosun Refractories BATN-D2, Lower Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | |
Chosun Refractories CRAZ-L43 Shroud Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | |
Chosun Refractories CUN-846 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | |
Chosun Refractories SB65S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.70 g/cc | >= 0.0975 lb/in³ | |
China-Yixing Longly Refractories Seggar Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Bulk Density | 2.70 - 2.95 g/cc | 0.0975 - 0.107 lb/in³ | |
China-Yixing Longly Refractories Shelf Boards and Pillars SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | Powder |
Ametek P316L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | Powder |
Ametek P316L P/M Stainless Steel, Sintered from 6.30 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Bulk Density | 2.70 g/cc | 0.0975 lb/in³ | Powder |