Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material
Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any..
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund..
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 Moldable Refractory Material
Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an..
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material
Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed ..
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
Chosun Refractories BATN-D2, Lower Gas Purging Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
Chosun Refractories CUN-846 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable
Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply ..