Chosun Refractories CUN-846 Nozzle Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CUN-846 Nozzle Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.70 - 2.80 g/cc
0.0975 - 0.101 lb/in³
Porosity 5.0 - 9.0 %
5.0 - 9.0 %
Mechanical Properties Metric English Comments
Compressive Strength <= 98.1 MPa
<= 14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.00 - 8.50 µm/m-°C

@Temperature 1000 °C
2.22 - 4.72 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 78 - 83 %
78 - 83 %
Carbon, C 3.0 - 5.0 %
3.0 - 5.0 %
Descriptive Properties Value Comments
Remarks Corrosion resistance, Spalling resistance