Material Notes:
P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L include enhanced compressibility, and green strength, which is approximately 40% higher than comparables induction melted materials.For property data reported here: Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintering in hydrogen vs. ammonia reduces strength and increases elongation. Compacting pressure 30 tsi. Green strength 400 psi. Sintered breaking strength 75,000 psi.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Bulk Density 2.70 g/cc
0.0975 lb/in³
Powder
Density 6.35 g/cc
0.229 lb/in³
Sintered
Mechanical Properties Metric English Comments
Hardness, Rockwell B 41
41
Tensile Strength, Ultimate 290 MPa
42000 psi
Elongation at Break 3.6 %
3.6 %
Thermal Properties Metric English Comments
Shrinkage 0.53 %
0.53 %
versus die size
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe 61.895 - 72 %
61.895 - 72 %
As Remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
2.0 - 3.0 %
Nickel, Ni 10 - 14 %
10 - 14 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Descriptive Properties Value Comments
Powder Flow 30 sec/50 g