Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This high refractory ramming material contains several well defined corund.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 Moldable Refractory Material Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an.. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | |
Chosun Refractories BATN-D2, Lower Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | |
Chosun Refractories CUN-846 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 - 2.80 g/cc | 0.0975 - 0.101 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |